王瑞瑞,史伊林,夏文薇.3种一步法自酸蚀粘接剂固化后的吸水性和溶解性[J].口腔材料器械杂志,2016,25(4):173-176.
3种一步法自酸蚀粘接剂固化后的吸水性和溶解性
Water sorption and solubility of three one-step self-etch adhesives
投稿时间:2015-08-25  修订日期:2016-01-27
DOI:10.11752/j.kqcl.2016.04.02
中文关键词:  一步法自酸蚀粘接剂  吸水性  溶解性  HEMA  浸泡时间
英文关键词:One-step self-etch adhesives  Water sorption  Solubility  HEMA  Water-storage time
基金项目:上海市科学技术委员会项目(10JC1408800)
作者单位E-mail
王瑞瑞 上海交通大学医学院附属第九人民医院牙体牙髓科, 上海市口腔医学重点实验室, 上海 200011  
史伊林 上海交通大学医学院附属第九人民医院牙体牙髓科, 上海市口腔医学重点实验室, 上海 200011  
夏文薇 上海交通大学医学院附属第九人民医院牙体牙髓科, 上海市口腔医学重点实验室, 上海 200011 xwwall@sina.com 
摘要点击次数: 1357
全文下载次数: 1151
中文摘要:
      目的 比较3种市售的一步法自酸蚀粘接剂的吸水性及溶解性,为临床操作提供指导。方法 选择3种一步法自酸蚀粘接剂Adper Easy Bond(AEO)、Optibond All-in-one(OP)和BeautiBond(BB),各制备50个圆盘试件(直径为8.0mm,厚度为1.0mm),浸泡于去离子水中,并分组于不同浸泡时间段(1天、7天、30天、90天、180天),通过浸水前后质量变化测定其吸水值与溶解值。结果 在每个浸泡期,OP的吸水值、溶解值均为最高,AEO吸水值居中、溶解值最低,BB吸水值最低而溶解值居中,不同品牌粘接剂组间比较,差异均有统计学意义(P<0.05);3种粘接剂的溶解值均随时间延长显著增加,不同浸泡时间组内比较,差异均有统计学意义(P<0.05)。结论 3种市售的一步法自酸蚀粘接剂固化后的吸水性和溶解性明显不同,可能与其组成有关。
英文摘要:
      Objective The purpose of this study was to evaluate the water sorption(Wsp) and solubility (Wsl) of three different one-step self-etch adhesives and provide guidance for clinical operations. Methods Three kinds of commonly used one-step self-etch adhesives including Adper Easy Bond (AEO), Optibond All-in-one (OP) and BeautiBond (BB) were selected. After the solvent of each adhesive was evaporated, disk-shaped specimens (8.0 mm in diameter x 1 mm in thickness) were prepared and divided into five subgroups with 10 specimens in each subgroup according to the different water-storage time. After 1, 7, 30, 90 and 180 days of water-storage time, the disks were subjected to measurement of Wsp and Wsl by testing the quality changes before and after immersion in water. Results At different water-storage time, the Wsp of OP was the highest and then followed by AEO and BB, while the Wsl of AEO was the lowest, and then followed by BB and OP. There were significantly statistical differences in the Wsp and Wsl among different adhesives (P<0.05). Moreover, the Wsl of OP, BB and AEO was increased with the increase of storage time, and there were significantly statistical differences in the Wsl among different storage times (P<0.05). Conclusions There were significantly differences in the water sorption and solubility among three selected one-step self-etch adhesives in this study, and it seemed to be mainly influenced by the adhesive composition.